Two-Sided Milling for a Recessed Panel
The operator turns the panel over to show the two machined faces, then shows a second setup. The cavity and the opposite face need access from different orientations.
Chapters
Selected chapter: Panel overview
Engineering notes
Identify the faces and cavity surfaces that control wall thickness. Confirm the drawing references and inspection method with the manufacturer.
Related engineering knowledge
Transcript
This job was 300 yuan per part. Stock cost
10 and anodizing cost 20.
Tax was 40, leaving 230. We made two
parts.
Both parts took five hours, including
programming and machining.
I used the machine behind me. There was no
flatness requirement.
But the internal features and this wall
thickness have tolerances.
The vise held the part for two setups.
The front and back are finished.
What do you think of the job? What is a
fair hourly rate?